TY - JOUR
T1 - The first single source deposition of tin sulfide coatings on glass: aerosol-assisted chemical vapour deposition using [Sn(SCH2CH2S)(2)]
AU - Parkin, I P
AU - Price, L S
AU - Hibbert, T G
AU - Molloy, K C
N1 - ID number: ISI:000168268800028
PY - 2001
Y1 - 2001
N2 - Aerosol-assisted chemical vapour deposition of SnS has been achieved on glass substrates from the single source precursor [Sn(SCH2CH2S)(2)] at 400-550 degreesC. In the presence of H2S the precursor produces films of SnS2 at 350 degreesC, Sn2S3 at 400 degreesC and SnS at 500 degreesC. The tin sulfides were analysed by Raman (SnS2 312 and 215 cm(-1); Sn2S3 307, 251, 234, 183, 87, 71, 60, 52 and 36 cm(-1) and SnS 288, 220, 189, 163 and 96 cm(-1)), EDAX, SEM and band gap measurements (SnS 1.15 eV, SnS2 2.20 eV). Growth rates were of the order of 15 nm min(-1).
AB - Aerosol-assisted chemical vapour deposition of SnS has been achieved on glass substrates from the single source precursor [Sn(SCH2CH2S)(2)] at 400-550 degreesC. In the presence of H2S the precursor produces films of SnS2 at 350 degreesC, Sn2S3 at 400 degreesC and SnS at 500 degreesC. The tin sulfides were analysed by Raman (SnS2 312 and 215 cm(-1); Sn2S3 307, 251, 234, 183, 87, 71, 60, 52 and 36 cm(-1) and SnS 288, 220, 189, 163 and 96 cm(-1)), EDAX, SEM and band gap measurements (SnS 1.15 eV, SnS2 2.20 eV). Growth rates were of the order of 15 nm min(-1).
M3 - Article
SN - 0959-9428
VL - 11
SP - 1486
EP - 1490
JO - Journal of Materials Chemistry
JF - Journal of Materials Chemistry
IS - 5
ER -