Abstract
As lithium-ion battery demand grows, so do fire safety challenges. Despite this, research on fire-damaged (FD) batteries remains limited. This study explores the distribution of valuable metals (such as Ni, Mn, Co, Cu) in two types of waste derived from lithium-ion nickel-manganese-cobalt oxide batteries (NMC811): black mass (BM) and FD waste. It emphasises that cobalt, manganese, and nickel-rich NMC811 particles are predominantly found in smaller particle size fractions (<125 µm), where they can account for up to 85% of total metal content. FD batteries show a similar, though less pronounced, trend. Evidence of structural degradation suggests that fire temperatures exceeded 500 °C; however, the presence of residual organic binders indicates that heat was unevenly distributed during the fire. FD batteries become friable and easily fragment into fine particles, which can hinder the effective separation of copper and aluminium current collectors, increasing their presence in processed material. The inclusion of FD batteries in standard BM processing introduces variability in output composition, potentially lowering the concentration of high-value NMC811 materials present. To maintain product quality and recycling output values, it is recommended that FD batteries are processed separately. Alternatively, particle size separation may allow for tailored outputs aligned with specific customer requirements.
| Original language | English |
|---|---|
| Article number | 034004 |
| Number of pages | 13 |
| Journal | Sustainability Science and Technology |
| Volume | 3 |
| Issue number | 3 |
| Early online date | 7 Jul 2026 |
| DOIs | |
| Publication status | Published - 1 Sept 2026 |
Data Availability Statement
All data that support the findings of this study are included within the article (and any supplementary information files).Acknowledgements
We gratefully acknowledge funding from the EPSRC ECR Fellowship NoRESt EP/S03711X/1 (W-AS, JB) and TReFCo EP/W019167/1 (W-AS, RC, DD, JB). The authors would like to thank the access to characterisation equipment to Swansea University Advanced Imaging of Materials (AIM) facility, which was funded in part by the EPSRC (EP/M028267/1) and the European Regional Development Fund throughthe Welsh Government (80708).
Funding
We gratefully acknowledge funding from the EPSRC ECR Fellowship NoRESt EP/S03711X/1 (W-AS, JB) and TReFCo EP/W019167/1 (W-AS, RC, DD, JB). The authors would like to thank the access to characterisation equipment to Swansea University Advanced Imaging of Materials (AIM) facility, which was funded in part by the EPSRC (EP/M028267/1) and the European Regional Development Fund through the Welsh Government (80708).
| Funders | Funder number |
|---|---|
| Engineering and Physical Sciences Research Council | EP/M028267/1 |
| EPSRC ECR Fellowship NoRESt | EP/S03711X/1 |
| TReFCo | EP/W019167/1 |
| European Regional Development Fund | 80708 |
UN SDGs
This output contributes to the following UN Sustainable Development Goals (SDGs)
-
SDG 7 Affordable and Clean Energy
Keywords
- end-of-life batteries
- fire-damaged batteries
- li-ion batteries
- NMC811
- thermal XRD
ASJC Scopus subject areas
- Renewable Energy, Sustainability and the Environment
- Environmental Science (miscellaneous)
- Engineering (miscellaneous)
- Materials Science (miscellaneous)
- Economics, Econometrics and Finance (miscellaneous)